非晶态U60Fe27.5Al12.5 合金的晶化动力学行为 |
| 韩录会, 柯海波, 张培, 桑革, 黄火根 |
|
Kinetic Crystallization Behavior of Amorphous U60Fe27.5Al12.5 Alloy |
| HAN Luhui, KE Haibo, ZHANG Pei, SANG Ge, HUANG Huogen |
| 图4 U60Fe27.5Al12.5非晶合金的ln[-ln(1 - x)]与1000 / T的关系,及局域动力学因子n(x)随x的演化 |
| Fig.4 ln[-ln(1 - x)] vs 1000 / T plots at various heating rates (a), and plots of local kinetic factor (n) as a function of x (b) of U60Fe27.5Al12.5 amorphous alloy |
|