非晶态U60Fe27.5Al12.5 合金的晶化动力学行为 |
| 韩录会, 柯海波, 张培, 桑革, 黄火根 |
|
Kinetic Crystallization Behavior of Amorphous U60Fe27.5Al12.5 Alloy |
| HAN Luhui, KE Haibo, ZHANG Pei, SANG Ge, HUANG Huogen |
| 图3 U60Fe27.5Al12.5非晶合金的-lnθ~1000 / T关系图及其晶化激活能Ec(x)随晶化体积分数的演化图 |
| Fig.3 The Ozawa plots of -lnθ vs 1000 / T at different x (a), and the activation energy |
|