Ag-CuO触点材料侵蚀过程的演化动力学及力学性能 |
| 马敏静, 屈银虎, 王哲, 王军, 杜丹 |
|
Dynamics Evolution and Mechanical Properties of the Erosion Process of Ag-CuO Contact Materials |
| MA Minjing, QU Yinhu, WANG Zhe, WANG Jun, DU Dan |
| 图7 岛状Ag-CuO和骨架Ag-CuO触点熔池表面的物相识别图及侵蚀层的三维模型图 |
| Fig.7 Phases identified diagrams and 3D morphologies of molten pool surface of island-restricted (a-c) and skeleton-restricted (d-f) Ag-CuO contacts (a, d) identified SEM images (The typical areas are highlighted in blue) (b, e) reverse reconstructed models (The typical areas are highlighted in yellow) (c, f) local pretreatment models |
|