Ag-CuO触点材料侵蚀过程的演化动力学及力学性能 |
| 马敏静, 屈银虎, 王哲, 王军, 杜丹 |
|
Dynamics Evolution and Mechanical Properties of the Erosion Process of Ag-CuO Contact Materials |
| MA Minjing, QU Yinhu, WANG Zhe, WANG Jun, DU Dan |
| 图6 1 × 104 cyc开断后触点垂直剖面的SEM像和模拟图 |
| Fig.6 Vertical section images of experimental (a, c) and simulated (b, d) island-restricted (a, b) and skeleton-restricted (c, d) Ag-CuO contacts after 1 × 104 make-and-break operations (w(Ag)—mass fraction of Ag) |
|