利用ZrO2 固体电解质研究Na3AlF6-SiO2 熔盐中的电沉积
|
|
高运明, 何林, 秦庆伟, 李光强
|
ZrO2 Solid Electrolyte Aided Investigation on Electrodeposition in Na3AlF6-SiO2 Melt
|
|
GAO Yunming, HE Lin, QIN Qingwei, LI Guangqiang
|
|
表2 对应于图5中各点位的EDS结果
|
Table 2 EDS results corresponding to the points in Fig.5
|
|
| Point | Mass fraction / % | Possible phase |
|---|
| (atomic fraction / %) |
|---|
| | | O | Ir | Zr | Au | | | | 1 | 25.97 | | 74.03 | | ZrO2 | | (66.67) | | (33.33) | | | | 2 | 3.56 | | 80.25 | 16.19 | Zr + ZrO2 | | (18.79) | | (74.27) | (6.94) | | | 3 | 25.97 | | 74.03 | | ZrO2 | | (66.67) | | (33.33) | | | | 4 | | 80.86 | 3.80 | 15.35 | Ir-Zr | | | (77.87) | (7.71) | (14.42) | | | 5 | | 79.34 | 8.18 | 12.48 | Ir-Zr | | | (72.96) | (15.84) | (11.20) | | | 6 | | 83.63 | | 16.37 | Ir | | | (83.97) | | (16.03) | | | 7 | 25.97 | | 74.03 | | ZrO2 | | (66.67) | | (33.33) | | |
|
|
|