利用ZrO2 固体电解质研究Na3AlF6-SiO2 熔盐中的电沉积 |
| 高运明, 何林, 秦庆伟, 李光强 |
|
ZrO2 Solid Electrolyte Aided Investigation on Electrodeposition in Na3AlF6-SiO2 Melt |
| GAO Yunming, HE Lin, QIN Qingwei, LI Guangqiang |
| 图6 Na3AlF6-5%SiO2熔盐在不同电位电解后电极Ir丝断面的SEM像及线扫描结果 |
| Fig.6 SEM images and scanline results of the Ir electrode section after electrolysis for Na3AlF6-5%SiO2 melt at constant potentials of -1.4 V (a), -1.6 V (b), -1.8 V (c), and -2.0 V (d) |
|