利用ZrO2 固体电解质研究Na3AlF6-SiO2 熔盐中的电沉积 |
| 高运明, 何林, 秦庆伟, 李光强 |
|
ZrO2 Solid Electrolyte Aided Investigation on Electrodeposition in Na3AlF6-SiO2 Melt |
| GAO Yunming, HE Lin, QIN Qingwei, LI Guangqiang |
| 图4 Na3AlF6-SiO2熔盐恒电位电解时电流随时间变化 |
| Fig.4 Curves of current vs time during potentiostatic electrolysis for Na3AlF6-SiO2 melt (RE: Pt, O2(air)|YSZ) |
|