利用ZrO2 固体电解质研究Na3AlF6-SiO2 熔盐中的电沉积 |
| 高运明, 何林, 秦庆伟, 李光强 |
|
ZrO2 Solid Electrolyte Aided Investigation on Electrodeposition in Na3AlF6-SiO2 Melt |
| GAO Yunming, HE Lin, QIN Qingwei, LI Guangqiang |
| 图5 纯Na3AlF6熔盐在-2.2 V电解后电极横断面及其附近和YSZ管底部沉积物的SEM像 |
| Fig.5 SEM images of cross section (a1) of the Ir electrode and local magnification (a2), sediment particles (b1) at the bottom of YSZ tube and local magnification (b2) after electrolysis for pure Na3AlF6 melt at -2.2 V |
|