形核剂的添加方式对选区激光熔化成形含锆Al-Cu-Mg合金显微组织与力学性能的影响 |
|||||||||||||||
| 王凯冬, 刘允中, 詹强坤, 黄斌 | |||||||||||||||
|
Effect of Adding Methods of Nucleating Agent on Microstructure and Mechanical Properties of Zr Modified Al-Cu-Mg Alloys Prepared by Selective Laser Melting |
|||||||||||||||
| WANG Kaidong, LIU Yunzhong, ZHAN Qiangkun, HUANG Bin | |||||||||||||||
| 表1 图10c中团聚相的EDS分析结果 (%) |
|||||||||||||||
| Table 1 EDS analysis results of agglomerated phases in Fig.10c |
|||||||||||||||
|
|||||||||||||||