显微组织和应变速率对TC4合金动态力学性能和绝热剪切带的影响 |
||||||||||||||||||||
| 陈伟, 章环, 牟娟, 朱正旺, 张海峰, 王沿东 | ||||||||||||||||||||
|
Effects of Microstructure and Strain Rate on Dynamic Mechanical Properties and Adiabatic Shear Band of TC4 Alloy |
||||||||||||||||||||
| CHEN Wei, ZHANG Huan, MU Juan, ZHU Zhengwang, ZHANG Haifeng, WANG Yandong | ||||||||||||||||||||
| 表1 不同组织TC4合金在不同剪切应变速率下的承载时间 (μs) |
||||||||||||||||||||
| Table 1 Bearing time of TC4 alloy with different microstructures at different shear strain rates |
||||||||||||||||||||
|
||||||||||||||||||||