显微组织和应变速率对TC4合金动态力学性能和绝热剪切带的影响 |
| 陈伟, 章环, 牟娟, 朱正旺, 张海峰, 王沿东 |
|
Effects of Microstructure and Strain Rate on Dynamic Mechanical Properties and Adiabatic Shear Band of TC4 Alloy |
| CHEN Wei, ZHANG Huan, MU Juan, ZHU Zhengwang, ZHANG Haifeng, WANG Yandong |
| 图7 不同组织TC4合金的绝热剪切带宽度变化曲线 |
| Fig.7 Variation curves of adiabatic shear band width (t) of TC4 alloy with different microstructures |
|