显微组织和应变速率对TC4合金动态力学性能和绝热剪切带的影响 |
| 陈伟, 章环, 牟娟, 朱正旺, 张海峰, 王沿东 |
|
Effects of Microstructure and Strain Rate on Dynamic Mechanical Properties and Adiabatic Shear Band of TC4 Alloy |
| CHEN Wei, ZHANG Huan, MU Juan, ZHU Zhengwang, ZHANG Haifeng, WANG Yandong |
| 图2 TC4合金原始试样和经过不同热处理后的XRD谱 |
| Fig.2 XRD spectra of TC4 alloy as-received and after different heat treatments |
|