成分对真空脱锰法相变控制高硅电工钢{100}织构的影响 |
| 杨平, 王金华, 马丹丹, 庞树芳, 崔凤娥 |
|
Influences of Composition on the Transformation-Controlled {100} Textures in High Silicon Electrical Steels Prepared by Mn-Removal Vacuum Annealing |
| YANG Ping, WANG Jinhua, MA Dandan, PANG Shufang, CUI Feng'e |
| 图1 4种合金热轧后(冷轧前)显微组织的OM像 |
| Fig.1 OM images of alloy 1 (a), alloy 2 (b), alloy 3 (c), and alloy 4 (d) after hot rolling (RD—rolling direction, ND—normal direction. White grains are ferrites, black regions are pearlites) |
|