2000℃高温高承载的Ta-W难熔合金 |
| 张旭, 田谨, 薛敏涛, 江峰, 李苏植, 张博召, 丁俊, 李小平, 马恩, 丁向东, 孙军 |
|
Ta-W Refractory Alloys with High Strength at 2000oC |
| ZHANG Xu, TIAN Jin, XUE Mintao, JIANG Feng, LI Suzhi, ZHANG Bozhao, DING Jun, LI Xiaoping, MA En, DING Xiangdong, SUN Jun |
| 图5 Ta-W合金25和2000℃高温压缩性能,以及该合金与文献中Ta-W合金[ |
| Fig.5 Compressive engineering stress-strain curves of Ta-W alloys at 25oC (a) and 2000oC (b), temper-ature dependence of compressive yield strength of Ta-W alloys in this work, Ta-W alloys[ |
|