连铸结晶器内高温熔体多相流模型化研究进展 |
| 刘中秋, 李宝宽, 肖丽俊, 干勇 |
|
Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold |
| LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong |
| 图14 结晶器内钢液-Ar气两相瞬态流场特征[ |
| Fig.14 Characteristics of molten steel-argon gas two-phase transient flow field in the mold[ Color online (a) RANS (b) LES (c) comparison of numerical simulation with experiment ( |
|