连铸结晶器内高温熔体多相流模型化研究进展 |
| 刘中秋, 李宝宽, 肖丽俊, 干勇 |
|
Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold |
| LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong |
| 图11 底部视角下的气泡聚并过程[ |
| Fig.11 Transient dumbbell coalescence process from a bottom view[ (a) experiment (b) numerical simulation (DPM—discrete phase model, ICM—interface-capturing model) |
|