连铸结晶器内高温熔体多相流模型化研究进展 |
| 刘中秋, 李宝宽, 肖丽俊, 干勇 |
|
Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold |
| LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong |
| 图10 数值模拟捕捉到的漩涡卷渣现象[ |
| Fig.10 Vortex slag entrapment phenomenon predicted by numerical simulation[ (a) interface of slag and steel (b) 20 mm below the slag-steel interface (c) flow field in the mold |
|