连铸结晶器内高温熔体多相流模型化研究进展 |
| 刘中秋, 李宝宽, 肖丽俊, 干勇 |
|
Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold |
| LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong |
| 图5 夹杂物在凝固坯壳上的捕捉位置[ |
| Fig.5 Locations of captured inclusions on solidified shell[ (a) 1.5 s (b) 3.0 s (c) 10 s (d) 30 s (e) 100 s |
|