激光增材制造过程中循环热输入对组织和性能的影响 |
| 王迪, 黄锦辉, 谭超林, 杨永强 |
|
Review on Effects of Cyclic Thermal Input on Microstructure and Property of Materials in Laser Additive Manufacturing |
| WANG Di, HUANG Jinhui, TAN Chaolin, YANG Yongqiang |
| 图7 原位析出强化和局部微观结构控制工艺原理[ |
| Fig.7 Principle of in-situ precipitation strengthening and local microstructure control process[ (a) real-time thermal history[ (b) layered structure diagram[ (c) secondary electron micrographs of soft and hard areas[ (d) atom probe tomography (APT) analysis of the soft and hard zones[ (e) microstructure with 30 s IDT[ (f) microstructure with 250 s IDT[ |
|