激光增材制造过程中循环热输入对组织和性能的影响 |
| 王迪, 黄锦辉, 谭超林, 杨永强 |
|
Review on Effects of Cyclic Thermal Input on Microstructure and Property of Materials in Laser Additive Manufacturing |
| WANG Di, HUANG Jinhui, TAN Chaolin, YANG Yongqiang |
| 图6 常见的激光扫描策略及扫描策略对组织织构的影响[ |
| Fig.6 A summary of laser scan strategies (a) and the effect of laser scan strategies on crystal orientations (b)[ |
|