数据驱动镍基铸造高温合金设计及复杂铸件精确成形 |
| 汪东红, 孙锋, 疏达, 陈晶阳, 肖程波, 孙宝德 |
|
Data-Driven Design of Cast Nickel-Based Superalloy and Precision Forming of Complex Castings |
| WANG Donghong, SUN Feng, SHU Da, CHEN Jingyang, XIAO Chengbo, SUN Baode |
| 图12 蜡模注射成型工艺参数之间的关系矩阵 |
| Fig.12 The relation matrix among the process parameters of wax pattern |
|