数据驱动镍基铸造高温合金设计及复杂铸件精确成形 |
| 汪东红, 孙锋, 疏达, 陈晶阳, 肖程波, 孙宝德 |
|
Data-Driven Design of Cast Nickel-Based Superalloy and Precision Forming of Complex Castings |
| WANG Donghong, SUN Feng, SHU Da, CHEN Jingyang, XIAO Chengbo, SUN Baode |
| 图8 Alloy 1和Alloy 2的SEM像 |
| Fig.8 SEM images of Alloy 1 (a, b) and Alloy 2 (c, d) (a, c) as-cast (b, d) after solid solution |
|