数据驱动镍基铸造高温合金设计及复杂铸件精确成形 |
| 汪东红, 孙锋, 疏达, 陈晶阳, 肖程波, 孙宝德 |
|
Data-Driven Design of Cast Nickel-Based Superalloy and Precision Forming of Complex Castings |
| WANG Donghong, SUN Feng, SHU Da, CHEN Jingyang, XIAO Chengbo, SUN Baode |
| 图7 筛选合金与几种典型铸造合金蠕变性能对比(JMatPro模拟结果) |
| Fig.7 Creep performance of screened alloys and several typical cast superalloys (evaluated by JMatPro) |
|