数据驱动镍基铸造高温合金设计及复杂铸件精确成形 |
| 汪东红, 孙锋, 疏达, 陈晶阳, 肖程波, 孙宝德 |
|
Data-Driven Design of Cast Nickel-Based Superalloy and Precision Forming of Complex Castings |
| WANG Donghong, SUN Feng, SHU Da, CHEN Jingyang, XIAO Chengbo, SUN Baode |
| 图1 新型镍基铸造高温合金热动力学模拟软件系统框架 |
| Fig.1 Framework of thermodynamic/kinetic simulation software for novel cast nickel-based superalloys |
|