析出强化Fe53Mn15Ni15Cr10Al4Ti2C1 高熵合金强韧化机制 |
| 孙士杰, 田艳中, 张哲峰 |
|
Strengthening and Toughening Mechanisms of Precipitation- Hardened Fe53Mn15Ni15Cr10Al4Ti2C1 High-Entropy Alloy |
| SUN Shijie, TIAN Yanzhong, ZHANG Zhefeng |
| 图2 经不同热处理工艺后冷轧Fe53Mn15Ni15Cr10Al4Ti2-C1高熵合金板材的显微硬度 |
| Fig.2 Microhardnesses of the cold-rolling (CR) Fe53Mn15Ni15Cr10Al4Ti2C1 sheets at different heat treatment processes(a) annealing at different temperatures for 1 h(b) annealing at 873 and 923 K for different time |
|