纳米孪晶强化304奥氏体不锈钢的应变控制疲劳行为 |
| 潘庆松, 崔方, 陶乃镕, 卢磊 |
|
Strain-Controlled Fatigue Behavior of Nanotwin- Strengthened 304 Austenitic Stainless Steel |
| PAN Qingsong, CUI Fang, TAO Nairong, LU Lei |
| 图5 纳米孪晶强化304 SS在低塑性应变幅(0.05%)疲劳时的微观结构特征 |
| Fig.5 Bright-field TEM images of typical NT grain with intact twins (a) and detwinned structures in the vicinity of SRX grains in NT strengthened 304 SS fatigued at Δε pl / 2 of 0.05% (b), and TEM image of rectangle area in Fig.5b showing twin boundaries with steps and dislocation tangles in the twin interior (c) |
|