钢精炼过程非金属夹杂物演变与控制 |
| 朱苗勇, 邓志银 |
|
Evolution and Control of Non-Metallic Inclusions in Steel During Secondary Refining Process |
| ZHU Miaoyong, DENG Zhiyin |
| 图12 引流砂中TiO x -SiO2-Al2O3相的SEM像及EDS结果[ |
| Fig.12 SEM image of TiO x -SiO2-Al2O3 base phase in ladle filler sand grains (a) and EDS result (b)[ |
|