钢精炼过程非金属夹杂物演变与控制 |
| 朱苗勇, 邓志银 |
|
Evolution and Control of Non-Metallic Inclusions in Steel During Secondary Refining Process |
| ZHU Miaoyong, DENG Zhiyin |
| 图10 由FactSage计算的CaO-SiO2-Al2O3-5%MgO渣系等铝活度(10-4)曲线图(1600℃) [ |
| Fig.10 Iso-activity lines of Al (10-4) in CaO-SiO2-Al2O3-5%MgO system calculated by FactSage (1600oC) [ |
|