钢精炼过程非金属夹杂物演变与控制 |
| 朱苗勇, 邓志银 |
|
Evolution and Control of Non-Metallic Inclusions in Steel During Secondary Refining Process |
| ZHU Miaoyong, DENG Zhiyin |
| 图5 Ca处理后MgO·Al2O3夹杂物的SEM像及线扫描图[ |
| Fig.5 SEM image (a) and elemental line scans (b) of a MgO·Al2O3 inclusion after Ca treatment[ |
|