钢精炼过程非金属夹杂物演变与控制 |
| 朱苗勇, 邓志银 |
|
Evolution and Control of Non-Metallic Inclusions in Steel During Secondary Refining Process |
| ZHU Miaoyong, DENG Zhiyin |
| 图4 在氧化铝夹杂物边缘生成的尖晶石的面扫描图[ |
| Fig.4 Elemental mappings of spinel layer formed at the edge of an alumina inclusion[ |
|