高熵合金涂层研究进展 |
| 崔洪芝, 姜迪 |
|
Research Progress of High-Entropy Alloy Coatings |
| CUI Hongzhi, JIANG Di |
| 图3 高速火焰喷涂 Fe49.7Cr18Mn1.9Mo7.4W1.6B15.2C3.8Si2.4非晶涂层的SEM像[ |
| Fig.3 SEM images of the polished surface morphology for the high-velocity air fuel (HVAF)-sprayed Fe49.7Cr18Mn1.9Mo7.4W1.6-B15.2C3.8Si2.4 amorphous coating[ (a) secondary electron image (b) back scatter electron image (c) enlargement for the rectangle 1 in Fig.3b (d) enlargement for the rectangle 2 in Fig.3b |
|