李少杰, 金剑锋, 宋宇豪, 王明涛, 唐帅, 宗亚平, 秦高梧

Multimodal Microstructure of Mg-Gd-Y Alloy Through an Integrated Simulation of “Process-Structure-Property”
LI Shaojie, JIN Jianfeng, SONG Yuhao, WANG Mingtao, TANG Shuai, ZONG Yaping, QIN Gaowu
表2 GW83K镁合金相场模型中不同退火温度与退火时间的取值
Table 2 The values of annealing temperature and time in phase field models for GW83K Mg alloy
Model Annealing temperature Annealing time
No. K min
1 623 60
2 623 75
3 623 90
4 673 60
5 673 75
6 673 90
7 723 60
8 723 75
9 723 90