“工艺-组织-性能”模拟研究Mg-Gd-Y合金混晶组织
李少杰, 金剑锋, 宋宇豪, 王明涛, 唐帅, 宗亚平, 秦高梧

Multimodal Microstructure of Mg-Gd-Y Alloy Through an Integrated Simulation of “Process-Structure-Property”
LI Shaojie, JIN Jianfeng, SONG Yuhao, WANG Mingtao, TANG Shuai, ZONG Yaping, QIN Gaowu
图4 具有不同晶粒尺寸的单晶粒相GW83K镁合金的实验拉伸应力-应变曲线及其本构输入曲线
Fig.4 Experimental tensile stress-strain (σ-ε) curves and constitutive input curves for monolithic grain GW83K Mg alloy with different grain sizes
(a) experimental data[13,74] ( d ˉ —average grain size from experiment, d 1 g - d 6 g —grain size ranges of the grain-interior phases 1-6)
(b) constitutive inputs of grain-interior phases 1-6 ( g 1 i n - g 6 i n ) for finite element model