“工艺-组织-性能”模拟研究Mg-Gd-Y合金混晶组织
李少杰, 金剑锋, 宋宇豪, 王明涛, 唐帅, 宗亚平, 秦高梧

Multimodal Microstructure of Mg-Gd-Y Alloy Through an Integrated Simulation of “Process-Structure-Property”
LI Shaojie, JIN Jianfeng, SONG Yuhao, WANG Mingtao, TANG Shuai, ZONG Yaping, QIN Gaowu
图1 GW83K镁合金在623、673和723 K时的自由能成分点和拟合曲线
Fig.1 Free energy-component data of GW83K Mg alloy at 623, 673, and 723 K, and their fitting curves (c Gd—concentration of Gd)