Cr含量对FeCrCoSi永磁合金调幅分解组织及其性能的影响 |
| 项兆龙, 张林, XIN Yan, 安佰灵, NIU Rongmei, LU Jun, MARDANI Masoud, HAN Ke, 王恩刚 |
|
Effect of Cr Content on Microstructure of Spinodal Decomposition and Properties in FeCrCoSi Permanent Magnet Alloy |
| XIANG Zhaolong, ZHANG Lin, XIN Yan, AN Bailing, NIU Rongmei, LU Jun, MARDANI Masoud, HAN Ke, WANG Engang |
| 图7 不同Cr含量试样经分级回火后调幅组织中Fe、Cr、Co和Si元素EDS面扫描叠加图 |
| Fig.7 Superimposed EDS maps of Fe, Cr, Co, and Si after step aging in samples 20Cr-SA (a), 25Cr-SA (b), 30Cr-SA (c), and 35Cr-SA (d) |
|