Cr含量对FeCrCoSi永磁合金调幅分解组织及其性能的影响 |
| 项兆龙, 张林, XIN Yan, 安佰灵, NIU Rongmei, LU Jun, MARDANI Masoud, HAN Ke, 王恩刚 |
|
Effect of Cr Content on Microstructure of Spinodal Decomposition and Properties in FeCrCoSi Permanent Magnet Alloy |
| XIANG Zhaolong, ZHANG Lin, XIN Yan, AN Bailing, NIU Rongmei, LU Jun, MARDANI Masoud, HAN Ke, WANG Engang |
| 图4 试样35Cr-SA调幅组织在[001]方向的HAADF像 |
| Fig.4 HAADF images of spinodal decomposition of sample 35Cr-SA, as viewed along [001] direction (The upper insets show fast Fourier transform (FFT) of Figs.4a, b, and c, respectively. The lower insets show the intensity profile of values taken along the lines AB, CD, and EF, respectively) (a) α 1 and α 2 phases (b) α 1 phase (c) α 2 phase |
|