Cr含量对FeCrCoSi永磁合金调幅分解组织及其性能的影响 |
| 项兆龙, 张林, XIN Yan, 安佰灵, NIU Rongmei, LU Jun, MARDANI Masoud, HAN Ke, 王恩刚 |
|
Effect of Cr Content on Microstructure of Spinodal Decomposition and Properties in FeCrCoSi Permanent Magnet Alloy |
| XIANG Zhaolong, ZHANG Lin, XIN Yan, AN Bailing, NIU Rongmei, LU Jun, MARDANI Masoud, HAN Ke, WANG Engang |
| 图2 固溶处理和分级回火处理后不同Cr含量FeCrCoSi试样的XRD谱 |
| Fig.2 XRD spectra of solution-treated (a) and step-aged (b) FeCrCoSi samples with different contents of Cr |
|