冷喷涂Ni及镍基复合涂层研究进展 |
| 李文亚, 张正茂, 徐雅欣, 宋志国, 殷硕 |
|
Research Progress of Cold Sprayed Ni and Ni-Based Composite Coatings: A Review |
| LI Wenya, ZHANG Zhengmao, XU Yaxin, SONG Zhiguo, YIN Shuo |
| 图6 Ni涂层截面的EBSD表征[ (a) Euler angle diagram (b) pattern quality diagram in the same area as Fig.6a |
| Fig.6 EBSD characterizations of Ni coating section (N2; 600oC; 3.0 MPa)[ |
|