冷喷涂Ni及镍基复合涂层研究进展 |
| 李文亚, 张正茂, 徐雅欣, 宋志国, 殷硕 |
|
Research Progress of Cold Sprayed Ni and Ni-Based Composite Coatings: A Review |
| LI Wenya, ZHANG Zhengmao, XU Yaxin, SONG Zhiguo, YIN Shuo |
| 图5 冷喷涂Ni涂层显微组织的TEM像(粒子与粒子的边界用箭头标记)[ |
| Fig.5 TEM image of cold sprayed Ni coating (Particle-particle boundary is marked with arrow)[ |
|