冷喷涂Ni及镍基复合涂层研究进展 |
| 李文亚, 张正茂, 徐雅欣, 宋志国, 殷硕 |
|
Research Progress of Cold Sprayed Ni and Ni-Based Composite Coatings: A Review |
| LI Wenya, ZHANG Zhengmao, XU Yaxin, SONG Zhiguo, YIN Shuo |
| 图4 冷喷涂Al、Ni、Cu、Zn的碰撞速度和回弹系数(临界速度以上时,回弹系数为零)[ |
| Fig.4 Coefficients of restitution for Al, Ni, Cu, and Zn (The coefficient of restitution is equal to zero above the critical velocity)[ |
|