界面热力学与晶界相图的研究进展 |
| 胡标, 张华清, 张金, 杨明军, 杜勇, 赵冬冬 |
|
Progress in Interfacial Thermodynamics and Grain Boundary Complexion Diagram |
| HU Biao, ZHANG Huaqing, ZHANG Jin, YANG Mingjun, DU Yong, ZHAO Dongdong |
| 图11 Pt-Au体系700 K偏析等温线[ |