界面热力学与晶界相图的研究进展 |
| 胡标, 张华清, 张金, 杨明军, 杜勇, 赵冬冬 |
|
Progress in Interfacial Thermodynamics and Grain Boundary Complexion Diagram |
| HU Biao, ZHANG Huaqing, ZHANG Jin, YANG Mingjun, DU Yong, ZHAO Dongdong |
| 图3 bcc结构W中Σ5 (310)[001]晶界以及2种晶界相的共存和相转变行为[ |
| Fig.3 Coexistence and phase transformation of Σ5 (310)[001] grain boundary and two grain boundary phases in bcc structure W[ |
|