航空发动机热障涂层的CMAS腐蚀行为与防护方法 |
| 郭磊, 高远, 叶福兴, 张馨木 |
|
CMAS Corrosion Behavior and Protection Method of Thermal Barrier Coatings for Aeroengine |
| GUO Lei, GAO Yuan, YE Fuxing, ZHANG Xinmu |
| 图5 LaPO4/YSZ涂层在1250℃下CMAS腐蚀2和10 h后的截面微观形貌[ |
| Fig.5 Cross-sectional microstructures with low (a, c) and high (b, d) magnifications of LaPO4/YSZ coatings after CMAS attack at 1250oC for 2 h (a, b) and 10 h (c, d)[ |
|