航空发动机热障涂层的CMAS腐蚀行为与防护方法 |
| 郭磊, 高远, 叶福兴, 张馨木 |
|
CMAS Corrosion Behavior and Protection Method of Thermal Barrier Coatings for Aeroengine |
| GUO Lei, GAO Yuan, YE Fuxing, ZHANG Xinmu |
| 图4 热处理后Ti2AlC的截面和元素的EDS结果[ |
| Fig.4 Cross-sectional microstructures of Ti2AlC (a) and EDS results of Ca (b), Mg (c), Al (d), Ti (e), and O (f) elements[ |
|