图2 高温下CMAS (CaO、MgO、Al2O3和SiO2)对热障涂层(TBCs)的破坏[13,43]
Fig.2 Degradation of thermal barrier coatings (TBCs) by CMAS (CaO, MgO, Al2O3, and SiO2) at high temperatures(a) thermochemical degradation[43](b) thermomechanical degradation[13]