航空发动机热障涂层的CMAS腐蚀行为与防护方法 |
| 郭磊, 高远, 叶福兴, 张馨木 |
|
CMAS Corrosion Behavior and Protection Method of Thermal Barrier Coatings for Aeroengine |
| GUO Lei, GAO Yuan, YE Fuxing, ZHANG Xinmu |
| 图1 不同制备方法的氧化钇部分稳定氧化锆(YSZ)涂层截面微观结构[ |
| Fig.1 Cross-section microstructures of yttria partially stabilized zirconia (YSZ) coatings by different preparation methods[ |
|