热电材料的载流子迁移率优化 |
| 赵立东, 王思宁, 肖钰 |
|
Carrier Mobility Optimization in Thermoelectric Materials |
| ZHAO Li-Dong, WANG Sining, XIAO Yu |
| 图7 能带锐化提升载流子迁移率与热电性能 (a) schematic of the relationship between band sharpening and carrier mobility (b) μ as a function of n (c) B as a function of T (d) ZT as a function of T |
| Fig.7 Strategy of band sharpening ((Pb1-xSnx)(Te1-xSex)[ |
|