钕铁硼永磁晶界扩散技术和理论发展的几个问题 |
| 刘仲武, 何家毅 |
|
Several Issues on the Development of Grain Boundary Diffusion Process for Nd-Fe-B Permanent Magnets |
| LIU Zhongwu, HE Jiayi |
| 图15 Pr-Al-Cu合金扩散前后磁体的抗压曲线及断裂后的形貌[ |
| Fig.15 Stress-strain curves of the original and Pr-Al-Cu diffused magnets (a) and SEM image of the fracture morphology of Pr-Al-Cu diffused magnet (b)[ |
|