钕铁硼永磁晶界扩散技术和理论发展的几个问题 |
| 刘仲武, 何家毅 |
|
Several Issues on the Development of Grain Boundary Diffusion Process for Nd-Fe-B Permanent Magnets |
| LIU Zhongwu, HE Jiayi |
| 图14 原始磁体和Pr-Al-Cu、La-Al-Cu和Al-Cu扩散磁体的极化曲线及其腐蚀后的微观结构[ |
| Fig.14 Polarization curves of the original magnet and Pr-Al-Cu, La-Al-Cu, and Al-Cu diffused magnets (a) and their microstructures after corrosion (b-e) (The yellow arrows refer to pits)[ |
|