钕铁硼永磁晶界扩散技术和理论发展的几个问题 |
| 刘仲武, 何家毅 |
|
Several Issues on the Development of Grain Boundary Diffusion Process for Nd-Fe-B Permanent Magnets |
| LIU Zhongwu, HE Jiayi |
| 图10 ZnO晶界扩散原理图与不同工艺ZnO扩散处理前后的退磁曲线[ |
| Fig.10 Schematic illustration of GBD with ZnO (a) and demagnetization curves for sintered magnet and the magnets with ZnO diffusion (b)[ |
|